Slygard184
.
I would like to know how you did Both sides of the cells with Only 22 oz. that comes out to about .03 oz for each cell. I just made and used 2 qts of resin for one 36 cell panel of 3x4 cells.
Also I found out that you can also use the resin that they use for Surf Boards,and it has the uv protection. I buy it from a guy in Florida, one gallon ends up to be $50.00 . I did some panels and they came out good and its holding up in the cold 20 deg. outside, and then I bring them indoors to about 70 deg. And every thing is fine.
John
The glass area is 26x31
.
I would like to know how you did Both sides of the cells with Only 22 oz. that comes out to about .03 oz for each cell. I just made and used 2 qts of resin for one 36 cell panel of 3x4 cells.
Also I found out that you can also use the resin that they use for Surf Boards,and it has the uv protection. I buy it from a guy in Florida, one gallon ends up to be $50.00 . I did some panels and they came out good and its holding up in the cold 20 deg. outside, and then I bring them indoors to about 70 deg. And every thing is fine.
John
The glass area is 26x31